簡述: 100Cr6軸承鋼綜合性能良好,淬火和回火后,硬度高且均勻,耐磨性能好,接觸疲勞強度高。鋼的熱加工性好,球化退火后有良好的可切削性。100Cr6圓鋼價格 100Cr6鋼板 材質100Cr6軸承鋼 100Cr6是什么材料 100Cr6圓棒 100Cr6對應國標

產(chǎn)品詳情

標準: DIN 17350(1980) Tool Steels; Technical Conditions of Delivery
鋼組: Tool steels
Application: Lathe centres, drills, threading dies, milling cutters, reamers
特性
100Cr6軸承鋼綜合性能良好,淬火和回火后,硬度高且均勻,耐磨性能好,接觸疲勞強度高。鋼的熱加工性好,球化退火后有良好的可切削性。
100cr6軸承鋼,韌性較好,具有較好的回火穩(wěn)定性,熱處理時變形小。該鋼中碳化物分布均勻,不易析出碳化物網(wǎng),并易于正火消除,通過正火可以消除網(wǎng)狀以及粗片碳化物組織。但是抗壓強度和耐磨性不足,加工性較差。該鋼的表面殘余含碳量為0.6%—0.7%的脫碳層時,由于碳化物的減少使得表面層的過熱敏感性增大。經(jīng)正常加熱淬火以后表面硬度仍可以達到60—62HRC,但其抗彎強度卻下降40%—50%。表面層晶粒度達到7級,心部為10級。
該鋼鍛造性能良好,由于易脫碳,需要在中性氣氛或者保護氣氛爐中加熱。施以鍛熱調質處理,可以獲得細密的回火索氏體組織,簡化工藝,省時節(jié)電,既有良好的切削加工性能,又有理想的余熱處理組織。
該鋼受熱軟化溫度為320℃,淬透性比鉻鋼好,油淬淬硬性深度40—50mm。該鋼零保溫淬火韌化工藝,可以消除搓絲=板因常規(guī)淬火加熱氧化脫碳造成的早期失效,不均勻奧氏體修或可以細化馬氏體,搓火后得到隱晶馬氏體或者細針狀馬氏體,這種組織強韌性好。
用途
宜制作壁厚≤12mm、外徑≤250mm 的各種軸承套圈、鋼球直徑≤50mm、圓錐、球面滾子直徑≤22mm及所有尺寸的滾針;還可用于制造量具、模具、木工刀具。制造內(nèi)燃機。電機車、機床、拖拉機、軋鋼設備、鉆探機、鐵道車輛以及礦山機械等傳動軸上的鋼球、滾子和軸套等。

化學成份
碳 C :0.95~1.05
硅 Si:0.15~0.35
錳 Mn:0.25~0.45
硫 S :≤0.025
磷 P :≤0.025
鉻 Cr:1.40~1.65
鎳 Ni:允許殘余含量≤0.30
銅 Cu:允許殘余含量≤0.25
鉬 Mo:允許殘余含量≤0.08
注:允許殘余含量Ni+Cu≤0.50

熱處理規(guī)范:850~860℃淬火,油冷;160℃回火2h。
金相組織:回火馬氏體。

●交貨狀態(tài):以熱軋(鍛制)退火,不退火,退火剝皮鋼、冷拉(軋)圓鋼,磨光圓鋼、熱軋鋼管,退火剝皮鋼管、冷拉(軋)鋼管八種狀態(tài)交貨。


Standard: DIN 17350 (1980) Steels Tool; Conditions of Delivery Technical
Steel Group: steels Tool
Lathe centres drills, threading, dies milling, cutters reamers, Application:
Characteristic
100Cr6 bearing steel has good comprehensive properties, quenching and tempering, high hardness and uniform, good wear resistance, high contact fatigue strength. The hot workability of steel is good, and it has good machinability.
100Cr6 bearing steel, toughness is good, with good tempering stability, heat treatment deformation is small. The steel carbide distribution, not to the precipitation of carbide network and easy to be normalized to eliminate, by normalizing can remove the mesh and plate coarse carbides. However, the compressive strength and wear resistance, poor processing. The steel surface residual carbon content of 0.6%, 0.7% of the decarburized layer, due to the carbide due to the decrease of surface layer of overheating sensitivity increases. The surface hardness can reach 60 to 62HRC after the normal heating and quenching, but the bending strength is decreased by 40% - 50%. The grain size of the surface layer reaches 7, and the heart is 10.
The good performance of steel forging, due to decarburization, need to be heated in a neutral atmosphere or protective atmosphere furnace. Impose forging heat quenching and tempering treatment can obtain fine tempered sorbite martensite structure, simplify the process, saving the electricity, both good cutting performance, and ideal heat treatment microstructure.
The steel heat softening temperature of 320 DEG C, the hardenability of steel ratio, oil quenching hardening depth of 40 - 50mm. The steel zero time holding quenching toughening technique, can eliminate rub silk = plate for conventional quenching heating oxidation and decarbonization cause early failure, inhomogeneous austenite or martensite refinement can, rub fire after cryptocrystalline martensite or fine acicular martensite body, the strong organization good toughness.
Use
Should produce wall thickness is less than or equal to 12 mm, outer diameter is equal to or less than 250mm all bearing ring, ball diameter is less than or equal to 50mm, cone, spherical roller diameter is less than or equal to 22mm and all dimensions of needle roller; also can be used in the manufacture of measuring tools, moulds, woodworking tools. Manufacturing internal combustion engine. Motor car, machine tool, tractors, steel rolling equipment, drilling machine, railway vehicles and mining machinery transmission shaft of the steel ball, roller and shaft sleeve.
Chemical composition
Carbon:0.95 C ~ 1.05
Silicon Si:0.15 ~ 0.35
Mn Mn:0.25 ~ 0.45
Sulfur: S = 0.025
P: P = 0.025
Chrome Cr:1.40 ~ 1.65
Ni Ni: allow residual content less than 0.30
Cu: allow residual copper content is less than 0.25
Mo Mo: allow residual content less than 0.08
Note: allow residual content of Ni+Cu is less than or equal to 0.50
Heat treatment specification: 850 ~ 860 for quenching, oil cooling; 160 tempering 2h.
Microstructure: temper martensite.
] delivery state: hot rolled (forging) annealing, annealing, annealing steel skinning, cold drawing (rolling) round, polished steel, hot-rolled steel pipe, eight annealing peeling steel tube, cold drawn steel pipe (rolling) delivery.

上一個:沒資料

下一個:供應軸承鋼 圓鋼 板材

 

版權所有:蘇州倍徠斯金屬材料制品有限公司 備案號:蘇ICP備15026697號

友情鏈接:蘇州倍徠斯金屬材料制品有限公司  蘇州倍徠斯金屬材料制品有限公司

1
許先生
3
潘經(jīng)理
4
許經(jīng)理
在線客服